Abstract

In this study, we prepared high-performance printable, stretchable electrical conductor from waterborne polyurethane and micro-silver flakes. The solidification and thermal degradation were investigated using differential scanning calorimetry and thermogravimetric analysis methods. The electrical conductor achieved solidification by volatilizing and removing the free water. The thermal degradation mainly happened in the range of 250–450 °C caused by the pyrolysis of the polymeric matrix of polyurethane. The pyrolysis kinetic equations were obtained using the kinetic methods, e.g., dα/dt = e22.16(1 − α)0.78 α 0.13e(−149.14/RT) for the polyurethane, dα/dt = e22.76(1 − α)0.84 α 0.11e(−150.69/RT), dα/dt = e21.43(1 − α)0.77 α 0.06e(−143.77/RT), and dα/dt = e19.06(1 − α)0.75 α 0.12e(−130.53/RT) for the electrical conductor containing 80, 85, and 90 % mass percentage of micro-silver flakes, where α was the fractional extent conversion at a given time t (or a given temperature T). Their overall order of reaction was 0.91, 0.95, 0.83, and 0.87, respectively, less than 1, demonstrating the thermal degradation was a single, simple reaction.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.