Lithium aluminosilicate powder precursors of compositions Li2O:Al2O3:SiO2 as 1:1:2; and 1:1:3.11 were synthesized and sintered by the Spark Plasma Sintering technique. The sintering conditions were adjusted to obtain dense ceramic materials in an attempt to avoid the presence of a glassy phase. XRD and SEM images were employed for composition and microstructure characterization. The coefficient of thermal expansion of the sintered samples was studied down to cryogenic conditions. Rietveld quantification was performed with the use of an external standard. Pure β-eucryptite of different compositions in dense ceramic bodies was obtained with a negative expansion coefficient.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.