Abstract

The Vickers hardness of α-Si3N4 is higher than that of β-Si3N4. The erosive wear caused by solid particle impingement was tested for a series of hot pressed Si3N4 ceramics with different phase contents of Si3N4. The anti-erosive wear property of Si3N4 including α-phase was inferior to that of 100% β-Si3N4. The poor anti-erosive wear of Si3N4 including α-phase is due to its low fracture toughness (Kc) in spite of its high hardness (H). The erosion rate (V) of hot pressed Si3N4 is related to H and Kc by the equation V=e8.76H-0.27Kc-7.1, derived from multiple regression analysis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.