Abstract

The reliability and integrity of pre-tinned copper-clad printed circuit (PC) boards are serious concerns in the manufacture of electronic devices. The factors that influence the wetting during soldering of Cu are discussed. The results suggest that pre-tinning with a Pb-rich solder, such as 95Pb-5Sn, is preferred to pre-tinning with eutectic solder, since the latter can develop exposed intermetallics during aging that wet poorly. The results also confirm that the use of flux leads to carbon contamination in the solder.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.