Abstract

A research has been carried out, aiming to optimize the thermal activation of chabazite tuff. The thermogravimetric examination of the dehydration process has been carried out, as a function of several parameters, including tuff grain size (6–250 mesh), activation temperature (100–375 °C), heating rate (1–100 ° C min ), obtaining indications on the best conditions of use. The ability of chabazite tuff to store thermal energy has been confirmed, pointing out that effective activations in static conditions are possible in few (1–4) hours at temperatures no higher than 200 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.