Abstract

Abstract PbTiO3 thin films were fabricated by the spinning method in the sol-gel process. Films with thickness of 0.15 μm to 4.0μm were coated on doped silicon substrates, using a multiple deposition process. The processing yields highly reliable crack-free films with easy control of crystal structure and composition at firing temperature of 550 to 750 °C. The very fine grain size in PbTiO3 films was studied as a function of firing temoperature. The ferroelectric and dielectric properties of the films were investigated using metal-ferroelectric-semiconductor configaration, and were strongly dependent on the film thickness and the firing temperature. Good ferroelectric properties can be obtained in the films of thickness more than 2μm fired at 600-650 °C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.