When using 100% self-fluxed pellets in the blast furnace burden, top charged fluxes, especially the BOFslag, may cause irregularities in operation. The major reason has been theoretically attributed to the problematic slag formation in the furnace. As the melting of pellets is the first step of the slag formation process, the softening and melting properties of LKAB’s self-fluxed pellets with and without addition of fluxes are studied experimentally. The results show that the softening and melting properties of the two types of LKAB’s self-fluxed pellets are quite suitable for blast furnace operation. Contrarily, the melting-down characteristics of BOF-slag are variable and harmful to the slag formation under a reducing atmosphere. Adding 5% BOF-slag to the selffluxed pellets can considerably worsen the softening and melting properties of pellets. It can either increase the softening and melting temperature interval substantially or cause the precipitation of solid phases, mainly di-calcium silicates, in the slag. It is quite likely that the resulting slag will therefore become very viscous, even entirely blocking the melting down of the pellets up to a temperature 1 520°C.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.