Abstract

To evaluate high temperature properties of blast furnace burdens, a series of reduction under load tests was carried out under the conditions simulating blast furnace processes, using sinter, self-fluxed pellets and acid pellets.To investigate the softening and melting mechanism, structural analysis was conducted on those samples taken after interrupting the test.The results obtained are summarized as follows:(1) Generation of molten slag is involved in the assimilation process of slag during softening and melting of samples, and the basic path for this assimilation is considered to be toward the final composition (average gangue composition before reduction) along the direction expanding the liquid phase area with heating.(2) The difference in softening and melting behavior of these burden materials is directly due to the quantity of molten slag formed in the slag assimilation process. It is indirectly due to the differences in reducibility at about 1000°C in addition to the composition and volume of gangue before reduction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.