Abstract

This paper is describing an investigation of sodium lingo-sulfonate and sodium dodecyl-sulfate mixtures influence on zinc concentrates high temperature oxidative pressure leaching and zinc electro-winning. For this purpose, surfactants concentration at leaching tests was varied from 200 to 800 mg∙l-1. It was established that the maximum zinc extraction (99 %) at leaching was achieved in the presence of mixture containing 800 mg∙l-1 lignosulfonate and 200 mg∙l-1 sodium dodecyl-sulfate. Therefore, this mixture can be recommended for high temperature oxidative pressure leaching of zinc concentrates. Sulfur-sulfide pellets formation also was observed at a low lingo-sulfonate concentration (200 mg∙l-1) in a mixture with sodium dodecyl-sulfate. This phenomenon can lead to emergency shut down of autoclave. It was observed that the mixture usage of 800 mg∙l-1 lignosulfonate and 200 mg∙l-1 sodium dodecyl-sulfate had no significant impact on zinc current efficiency, it was in the rage of 92-93 %. The mixture usage of 200 mg∙l-1 lignosulfonate and 600 mg∙l-1 sodium dodecyl-sulfate allowed to increase current efficiency up to 95 %. Increasing sodium dodecyl-sulfate concentration in mixtures with lignosulfonates leads to decrease of current efficiency, to formation of deep pores and defects on cathode zinc surface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.