Influence of typical ceramic deflocculant – sodium hexametaphosphate – on the rheological properties (viscosity) of calcium aluminate cement paste, porcelain raw materials mixture (casting slip), and fired porcelain body respectively, was determined. It was used two different typed of calcium aluminate cements (from two sources – producers - Istra, Almatis) with different content of Al2O3 (40 % and 70 %). Sodium hexametaphosphate decreases of water content needed to prepare slip casting with constant viscosity. Deflocculant increases the modulus of rupture MOR of dried green body and its bulk density. Sodium hexametaphosphate admixture is very suitable for the creation of porcelain body with low porosity after firing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.