Abstract
The presence of Na in Cu(In,Ga)Se2 (CIGS) is well known to improve the solar cell performance. To incorporate Na into the CIGS absorber, Na-doped Mo (MoNa) back contact layers were grown on stainless steel foils. Three different back contact designs deposited from MoNa sputtering targets with Na concentrations of 3at.%, 5at.% and 10at.% were investigated. A multistage CIGS evaporation process at low (~450°C) substrate temperature was used to deposit the absorbers.Measurements from time-of-flight secondary ion mass spectroscopy depth profiles indicate that Na is preferentially collected at the internal interfaces and out-diffuses from the grain boundaries of the multilayer MoNa back contact into the CIGS absorber. From the [Ga]/([In]+[Ga]) grading profiles, a more pronounced Ga dip was found with increasing Na concentration. Moreover, at high Na concentrations (10at.% MoNa target), a change in the CIGS texture was observed by X-ray diffraction. Best solar cell efficiency of 14.4% was achieved for the 5at.% MoNa sample without antireflective coating, which is a significant improvement compared to the 9.8% efficiency measured for the Na-free reference.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.