Fresh water sponge was used as a silica source for the synthesis of MCM-41 via the hydrothermal process. The silica was extracted from the sponge by washing with nitric acid and piranha solution. Synthesis of MCM-41 was performed at 100 °C for 5 days and the procedure was optimized, with modifications made to the leaching temperature of the silica and the synthesis of mesoporous material, which was characterized by XRD, FT-IR, SEM and adsorption of N2. The optimal result was achieved at a temperature of 135 °C for 3 days, showing ordered mesoporous material with a surface area of 1080 m2 g-1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.