The size-dependent diamond-graphite phase transition was detected in the course of a study of the growth of nanosized diamond particles under conditions of thermal treatment at 8 GPa. It was found that a critical size of diamond nanoparticles, on reaching which they transformed into graphite, was reached at 1623 K and a treatment time of 60 s, and it was equal to ∼18 nm. The activation energy of the solid-phase growth of nanosized diamond particles at 8 GPa was determined to be 112±8 kJ/mol.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.