Solid state synthesis route was employed to form Ba0.85Ca0.15Zr0.1Ti0.9O3 powder. The calcined powder was high energy ball milled at different milling speeds to get powders of different particle sizes. XRD pattern of the ceramics made from these powders show the presence of pure perovskite. This paper deals with a systematic study of the pyroelectric and the fatigue properties of the ceramics. The room temperature pyroelectric coefficient (p) attains the minimum value p = 0.119X10−8 C cm−2 K−1 for the ceramic made from the powder milled at 250 rpm. The fatigue was also found to be minimum for the same ceramic samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.