Abstract
Sol-gel blends are created using a combination of a high refractive index (n∼2.4) TiO2 based sol-gel and a low refractive index (n∼1.5) SiO2 based sol-gel. The blends are prepared with different ratios of sol-gels and films are created using the spin coating method on silicon and ITO-on-glass substrates. The film thickness, refractive index, and dielectric constants of the resulting films are measured using profilometry, prism coupling, and LCR measurements, respectively. Results show that including more SiO2 based sol-gel in the initial mixture creates thicker films ranging from 1-7 μm, but results in lower refractive index and lower dielectric constants. This is consistent with expectations due to SiO2 having a lower refractive index and dielectric constant than titania over a range of wavelengths andfrequencies. The ability to fine tune the properties is explored.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.