Abstract

Effect of different additives, namely Cr2O3, Fe2O3 and TiO2, up to 2 wt% was studied on the sintering and microstructural developments of the chemically pure magnesia using the pressureless sintering technique between 1500 and 1600°C. Sintering was evaluated by per cent densification and microstructural developments were studied by electron microscopy and elemental distribution of the additives in the sintered products was also investigated for their distribution in the matrix. Cr2O3 and TiO2 were found to deteriorate the densification associated with grain growth. Fe2O3 was found to improve the densification and well-compacted grain distribution was observed in the microstructure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.