Abstract

In the composition of ZrO 2(8 mol% Y 2 O 3) Al 2 O 3 = (100−85) (0–15) mol% , metastable c-ZrO 2 solid solutions crystallize at low temperatures from amorphous materials prepared by the hydrazine method. Powders have been characterized. Crystallite size and specific surface area are strongly dependent on heating temperature. Hot isostatic pressing has been performed for 1 h at 1600°C under 196 MPa. Yttria-stabilized c-ZrO 2 materials with homogeneous-dispersed Al 2O 3 derived from the decomposition of solid solutions give >99% of theoretical densities. Materials with small amounts of Al 2O 3 show good strength and excellent high ionic conductivity at high temperatures.