Fe–4.5 wt.% Cu–1.75 wt.% Sn–1 wt.% MoS 2 antifriction material with varying additions of Pb (0.0–12.5 wt.%) were developed by a conventional powder metallurgy route by sintering at 800, 850 and 900°C for 20–50 min and the mechanical and frictional properties of the sintered compacts were evaluated. Addition of Pb up to 7.5 wt.% improved the antifrictional and mechanical properties, whereas further addition deteriorated these properties. The lowest coefficient of friction of 0.08 at the PV value of 0.76 MPa ms −1 and the maximum hardness level of 254 VHN were obtained for the composition containing 7.5 wt.% Pb sintered at 850°C for 30 min.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.