Abstract

Diamond powder can be successfully cemented with cobalt. At 62 kilobars the sintering occurs over the temperature range from 1570 degrees to 1610 degrees C. The maximum microhardness of the compact ( 3000 kilograms per square millimeter on the Knoop scale) is obtained with a mixture of 20 percent cobalt (by volume) and a diamond particle size of 1 to 5 micrometers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.