Ce(Co-Cu-Fe-Ti)z alloys were prepared with 5.6⩽z⩽7.4. They were ground into powders and sintered in Ar atmosphere. It was found that Ti enhanced coercivity and rectangularity. A permanent magnet with Br=7400 G, IHc=6100 Oe, (BH)max=13 MG Oe, and rectangular hysteresis loop was achieved on sintered samples having the composition Ce(Co0.727Fe0.12Cu0.14 Ti0.013)6.5.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.