Abstract

Cherenkov radiation (CR) in both the visible and mid-infrared regions is simultaneously generated experimentally based on a photonic crystal fiber with two zero-dispersion wavelengths. The generation of CR in the visible region originates from solitons located in the anomalous group velocity dispersion (GVD) regime which are perturbed by positive third order dispersion. Conversely, the generation of CR in the mid-infrared region requires that the solitons in the anomalous GVD regime are perturbed by negative third order dispersion. The peak wavelength of the CR in the visible region can be tuned from 498 to 425 nm by increasing the average input pump power from 70 to 400 mW, while the peak wavelength of the CR in the mid-infrared region can be tuned from 1986 to 2279 nm by increasing the average input pump power from 70 to 320 mW.