The simultaneous deactivation by coke and sulfur of monometallic Pt/Al 2O 3 and bimetallic Pt–Re(Ge, Sn)/Al 2O 3 catalysts was studied using n-hexane reforming as bifunctional test reaction and thiophene as poisoning molecule. The residual activities in the activity decay curves were used for measuring the catalyst sensitivity to coke formation and sulfur poisoning. Sulfur and carbonaceous deposits accumulated essentially on the metallic fraction and affected the catalyst activity for both monofunctional metallic and bifunctional metal–acid catalyzed reactions. The overall deactivation rate for n-hexane conversion increased in the order Pt–Ge<Pt⪡Pt–Sn≤Pt–Re. This deactivation trend resulted from the combination of the catalyst resistance to each individual deactivation process. Pt–Ge/Al 2O 3 was the most stable catalyst essentially because of its high thiotolerance for n-hexane transformation reactions and also because it showed low activity for dehydrogenation reactions leading to the formation of coke precursors. Sulfur poisoning on Pt/Al 2O 3 decreased monofunctional metal-catalyzed reactions but concomitantly increased the activity for acid-controlled skeletal rearrangement reactions; as a result, n-hexane conversion was only slightly diminished by the addition of sulfur. Pt–Sn/Al 2O 3 showed high resistance to coke deactivation but was severely poisoned by the addition of sulfur. The Pt–Re/Al 2O 3 activity was significantly decreased by both deactivation processes. Changes in catalyst selectivity are interpreted in terms of selective deactivation by coke and sulfur of individual reaction pathways involved in the n-hexane reforming mechanism.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call