Abstract

AbstractThe nickel‐rich superalloys Alloy 600 and Alloy 800 have been corroded in mildly alkaline deuterated aqueous conditions typical of secondary coolant circuits in a nuclear power station. The oxide films and substrates of these alloys have been analysed by imaging SIMS depth profiling, which makes it possible to describe elemental distribution in all three dimensions. The measurement of the distribution of the secondary ions NiO−, FeO− and CrO− appears useful for detailing the behaviour of nickel, iron and chromium within oxidized phases. The measurement of D− distribution outlines the extent of oxide hydration. For Alloy 800, evidence of sodium migration into the grain boundaries of the alloy substrate is found. For Alloy 600, no grain boundary sodium ingress can be identified under comparable corrosion conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.