Abstract

We report a simple, cost-effective, and environmentally benign process for reducing graphite oxide by treating solely with sulfuric acid. The suggested process consists of a two-step reduction of graphite oxide, first in aqueous sulfuric acid at room temperature and then in concentrated sulfuric acid with refluxing. X-ray diffractometry, X-ray photoelectron spectroscopy, Raman spectroscopy and thermogravimetric analysis demonstrated that the graphite oxide was reduced effectively and was comparable in composition to reduced graphite oxide prepared using previously described methods that rely on toxic and hazardous reducing agents, such as hydrazine, sodium borohydride, or hydrohalic acids.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.