In the present study, we sought to develop materials applicable to personal and collective protection equipment to mitigate SARS-CoV-2. For this purpose, AgNPs were synthesized and stabilized into electrospinning nanofiber matrices (NMs) consisting of poly(vinyl alcohol) (PVA), chitosan (CHT), and poly-ε-caprolactone (PCL). Uniaxial nanofibers of PVA and PVA/CHT were developed, as well as coaxial nanofibers of PCL[PVA/CHT], in which the PCL works as a shell and the blend as a core. A crucial aspect of the present study is the in situ synthesis of AgNPs using PVA as a reducing and stabilizing agent. This process presents few steps, no additional toxic reducing agents, and avoids the postloading of drugs or the posttreatment of NM use. In general, the in situ synthesized AgNPs had an average size of 11.6 nm, and the incorporated nanofibers had a diameter in the range of 300 nm, with high uniformity and low polydispersity. The NM's spectroscopic, thermal, and mechanical properties were appropriate for the intended application. Uniaxial (PVA/AgNPs and PVA/CHT/AgNPs) and coaxial (PCL[PVA/CHT/AgNPs]) NMs presented virucidal activity (log's reduction ≥ 5) against mouse hepatitis virus (MHV-3) genus Betacoronavirus strains. In addition to that, the NMs did not present cytotoxicity against fibroblast cells (L929 ATCC® CCL-1TM lineage).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.