Abstract
Structurally perfect, high-purity silicon epilayers up to 20 μm in thickness, with a carrier concentration n = 1012 cm−3 are grown through thermal decomposition of silane. Experimental evidence is presented that the concentration of “electrically active” impurities in high-purity silane can be evaluated from the electrical parameters of Si epilayers grown from it.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.