Abstract

In the present study, a zirconia-based primary slurry free from silica (S-0) was prepared by replacing the colloidal silica sol binder in the commercial zirconia-based slurry (S-6.4) with an aqueous polymer binder. The results of X-ray diffraction (XRD), scanning electron microscopy (SEM), and line scan analyses from the surface of cast samples show that the thickness of reaction layer has been decreased from 10 to 6 µm in the samples S-6.4 and S-0, respectively. Also, the microhardness tests obtained from the sample surfaces show a 80 µm decrease in the surface-hardened layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.