High-yield wafer bonding with minimal bonding imperfections and high-aspect etch process of 4H-SiC/SiO2/4H-SiC stacks is presented. The top 4H-SiC layer is thinned, patterned, etched, and is then ready to be released to form the MEMS device layer. An anti-bosch process is used to etch high aspect ratio trenches within the 4H-SiC device layer in the presence of buried oxide; the oxide serves both as a sacrificial layer and as an etch stop. The etch yields an aspect ratio of 10.5 (42.9 μm etch depth : 4.1 μm mask opening) within the 4H-SiC device layer. The handle wafer is 4H-SiC, as opposed to Si, which allows for all SiC-based MEMS devices for high shock resistant and temperature applications.