Abstract
The aim of this study was to investigate the micro tensile bond strength of a self-etch adhesive system following 1 year storage in water. 10 sound human molar teeth were used for micro tensile bond strength test. Twostep self-etch dentin adhesive (Clearfil SE Bond®) was applied to the flat dentin surfaces according to the manufacturer's instructions. Composite blocks (Z- 250; 3M ESPE) of 5 mm in height have been prepared by using layering technique. Teeth were stored in water for 24 hours at 37°C and longitudinally sectioned to obtain dentin sticks of 1 mm2.Randomly selected samples from half of the teeth were immediately subjected to micro tensile test and. Remaining specimens were tested after 1 year storage in water. Bond strengths were calculated in megapascal (MPa). Means and standard deviations of the Clearfil SE Bond® micro tensile bond strength values were, respectively, 37.31 ± 13.77 MPa and 24.78 ± 2.99 MPa after 24 h and 1 year of storage in water. The difference was statistically significant (p=0.031). Long-term storage in water decreased the micro tensile bond strength values of the twostep self-etch adhesive which has been accepted as the gold standard in bond strength tests.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Istanbul University Faculty of Dentistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.