The shape fixity and recoverability in a thin film of shape memory polymer of the polyurethane series were investigated using the thermomechanical cycling tests with loadings at various temperatures. The results are summarized as follows. (1) During the heating process under no load, strain is recovered at temperatures in the vicinity of the glass transition temperature Tg in the case of loadings at Tg and Tg+20K, but in the case of loadings at Tg-20K it is recovered at temperatures in the vicinity of Tmg. (2) The rate of strain recovery is about 98%, except for the early cycles in the case of loadings at Tg and Tg+20K, while it decreases with increasing cycles in the case of loading at Tg-20K. (4) The thermomechanical properties of materials with different Tg are quite alike in spite of the difference in Tg.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: TRANSACTIONS OF THE JAPAN SOCIETY OF MECHANICAL ENGINEERS Series A
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.