This study aims to determine the effect of precursor and activator proportion on the setting time of the geopolymer binder. The precursor used was Umeanyar slate stone powder containing SiO2 (49%), Al2O3 (11%), CaO (11.2%). While the activator used was a mixture of 14 M sodium hydroxide (NaOH) solution and sodium silicate (Na2SiO3). The proportion of precursor: activator (P/A) in the geopolymer binder were 70%: 30%; 75%: 25%; 80%: 20% and those of Na2SiO3 : NaOH (SS/SH) were 1:1; 1.5:1; 2:1, by weight. The setting time of the binders was tested according to the SNI 2049: 2015. Measurement of setting time using vicat test equipment and based on normal consistency. The measurement of the setting time was carried out every 15 minutes until the initial bonding time was reached. The initial and final setting time result of the geopolymer binder decreased to 75 minutes and 100 minutes when P/A, as well as, SS/SH increased.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.