The low-grade nickel laterite ore used in this study was successfully upgraded through selective reduction by industrialized rotary kilns followed by magnetic separation. The results indicated that both iron metallization extent and nickel metallization extent showed obvious linear correlation. In addition, rational roasting temperature and prolonged grinding time could enhance the overall fineness level of reduced laterite nickel ore. The moderate roasting temperature at a range of 1100–1150 °C should be suitable enough to a conversion of total nickel to metallic nickel and partly inhibited the conversion of total iron. Ultimately, the obtained ferronickel alloy with a nickel content of 7.32% and an iron content of 84.15% was prepared successfully from the low-grade nickel laterite ore containing a nickel content of 1.92%. Nickel and iron recoveries were 96.72 and 89.08% respectively, which achieved the highly efficient recovery and utilization of iron and nickel from low-grade laterite nickel ore.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.