Ten compositions were prepared in the systems As:Se:Te and As:S:Te. Nine of these compositions were amorphous in structure. The resistivities and Seebeck coefficients of these materials were measured as functions of temperature. The resistivity varied exponentially with temperature, while the Seebeck coefficient varied linearly. At 298°K, the resistivity values for the amorphous samples ranged from 4.7×104−2.5×1013 ohm-cm, while the Seebeck coefficient values ranged from 830–1625 μv/°K (p type). At any temperature, the resistivity decreased with increase in tellurium content. For the amorphous materials, the thermal conductivity values ranged from 2.4–4.4 mw/cm-°K.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.