Abstract

The Cu/ZSM-5, Ce/ZSM-5 and Cu-Ce/ZSM-5 catalysts were prepared and characterized in this investigation and the catalytic activity of carbon monoxide (CO) combustion under these catalysts was determined by temperature-programmed oxidation. The activity for the CO combustion follows the decreasing order: Cu-Ce/ZSM-5>Cu/ZSM-5>Ce/ZSM-5, indicated by lower ignition, light-off, extinction temperature and broader hysteresis determined via both heating and cooling feeding process. The CO adsorbed on the copper sites to form Cu+–CO complexes, monodentate and bidentate carbonates was considered to be the crucial step for CO catalytic combustion. At the CO concentration ≥5vol.%, the CO self-sustained combustion was achieved over the Cu-Ce/ZSM-5 catalyst. One reason is due to formation of Cu2+ ions incorporated into cerium oxides, which are more reducible than the copper clusters, minicrystals and bulk CuO particles. Another reason is attributable to the formation of Ce4+/Ce3+ redox couple, which facilitates oxygen transport on the catalyst surface.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call