Highly densified Nd-bearing Y2Ti2O7 pyrochlores were prepared within 5min by self-propagating high-temperature synthesis plus quick pressing (SHS/QP) using Fe2O3 as the oxidant. As the surrogate of trivalent actinides, Nd was introduced to substitute the Y site with nominal formulation of Y2−xNdxTi2O7. The ordered pyrochlore phase was generated as the main ceramic phase with x≤1.0. Phase separation of Nd-rich and Y-rich phases is formed in the pyrochlore matrix. The pyrochlore-base waste form (Nd0.5) demonstrates promising aqueous durability. The 42days normalized leaching rates of Y and Nd are calculated to be 2.59×10−5 and 2.80×10−5gm−2d−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.