Abstract

Rapid methods for assessing the fatigue properties of materials have been developed, among which the self-heating method stands out as particularly promising. This approach analyzes the thermal signal of the specimen when subjected to cyclic loading. In this research, the self-heating method was utilized for the first time with laser powder bed fusion (LPBF) of NiTi alloys, examining two specific loading conditions: loading ratios of 0.1 and 10. A thorough examination of the material self-heating behavior was conducted. For comparative purposes, conventional fatigue tests were also conducted, alongside interrupted fatigue tests designed to highlight the underlying mechanisms involved in high cycle fatigue and potentially self-heating behavior. The investigation revealed several key mechanisms at play, including intra-grain misorientation, the emergence and growth of persistent slip bands, and the formation of stress-induced martensite. These findings not only deepen our understanding of the fatigue behavior of LPBF NiTi alloys but also highlight the self-heating method potential as a tool for studying material fatigue.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call