Abstract

Selective Laser Melting (SLM) was used to process a powder mixture of CP Ti, 6.5 wt% Mo and 3.5 wt% Mo2C. The process parameters were optimized to obtain full-density, crack free parts. After the in situ decomposition of Mo2C in favor of the formation of TiC, the material consisted of a homogeneous dispersion of submicrometer sized TiC platelets in a β-(Ti,Mo) matrix exhibiting a high hardness up to 550 HV and compressive yield stress of 1164 ± 37 MPa. The microstructure and mechanical properties could be tailored by variation of the process parameters within the high-density processing window, as well as through post-process heat treatments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.