Abstract
Pure magnesium (Mg) is widely used as biomedical material, but its degradation rate is often too high and problematic to clinic applications. In this study, selective laser melting (SLM) was used to prepare an Fe-based metallic glass surface on a pure Mg substrate, forming a hybrid material to explore the advantage associated with such designed structure. It was found that the corrosion resistance was significantly improved with the hybrid material (from 0.89 ± 0.1 mm/a to 0.11 ± 0.03 mm/a in simulated body fluid), along with much increased hardness from 0.46 GPa to 14.3 GPa. The metallic glass surface was shown to retain its amorphous nature after the SLM processing. The molten pool formed by the applied laser beam resulted in a good mechanically interlocked bonding between the metallic glass layer and the Mg matrix. It was further revealed that the metallic glass surface had better wetting property than the Mg substrate, explaining why the MG-63 cells had good adhesion to it. The cell toxicity test was followed under the in vitro condition, indicating no toxicity in the metallic glass part. The results provide a feasible way to develop advanced Mg materials for biomedical applications via the capable SLM technology and via the suggested hybrid material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.