Abstract

This paper focuses on two innovative bond technologies, which enable a selective heating of the bond interface only. The reactive bonding with the new CuO/Al multilayer system could by successfully used for wafer bonding. With a tool pressure of 0.5 to 5 bar an average shear strength of 64 N/mm² for Si-glass and 143 N/mm² for Si-Si could be reached. The bond time is < 1 s due reaction velocities of 28 m/s to 40 m/s. The focus of inductive bonding is the support and enhancement of the solid-liquid interdiffusion (SLID) process at wafer level by using selective and energy-efficient induction heating of Cu-Sn layers. With IR thermography, the heat distribution and the achieved heating rate of approx. ∆T = 150 K/s could be investigated. By applying a tool pressure of 2 MPa and a bond time of 120 s an average shear strength of 68 N/mm² could be achieved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.