To prevent the oxidation of BN-coated sapphire optical fiber (SOF) at 800 °C, a SiBCN ceramic coating was used as an outer coating owing to its excellent high-temperature oxidation resistance. Compared with BN/SOF, the tensile strength of SiBCN/BN/SOF increases from 500 to 723 MPa at 1200 °C. The optical properties of double coating indicate that the addition of SiBCN does not diminish the total reflection of the BN coating. Furthermore, SiBCN-coated fibers indicate lower residual stress and performed better compared with other coated fibers in terms of mechanical and optical properties. Hence, SiBCN is highly suitable as an outer coating of SOF.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.