Abstract

Immersion of glass ionomer cement (GIC) type II in acid drink like isotonic drink could reduce its compressive strength.This is due to the matrix degradation process of GIC in acid condition. However, there is artificial saliva that canneutralize this condition. The purpose of this study was to evaluate the effect of artificial saliva on compressive strengthof glass ionomer cement type II immersed in isotonic drink. The GICspecimens of 6 x 6 x 12 mm3beam were immersed for24 hours in distilled water, 24 hours in isotonic drink, 24 hours in isotonic drink continued with 72 hours in artificial saliva,48 hours in isotonic drink, and 48 hours in isotonic drink continued with 144 hours in artificial saliva. The compressivestrength was measured using Universal Testing Machine with a crosshead speed of 0.5 mm/min. Statistical analysis wasperformed by one-way ANOVA and post-hoc LSD test (=0.05) showed a significant difference of compressive strength(p<0,05). It was concluded that artificial saliva increases the compressive strength of GIC immersed in isotonic drink.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.