Abstract
The polyester fiber was utilized to fabricate the woven spacer fabric on the common loom, and the sandwich panels were produced by resin transfer molding process (RTM). The parameter of RTM molding process was determined. The correct ratio of resin, curing agent and accelerator in RTM process is 100:86:1. The injection temperature is 65°C. Injection time is shorter than 2 hours. Flexure and flatwise compression of composite panels were tested. The experiment result shows: flexure property and flatwise compression property of the RTM composite panels are better than that produced by handle paste shaping process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.