Abstract

Deep penetration laser welding is promising in joining thick (> 10 mm) steel sections. Focused laser beam by drilling vapour cavity, the keyhole, generates deep and narrow welds. Full penetration single-pass joining has a persistent problem with root quality where humping is one of the most frequent imperfection. This strongly hampers the use of high-power laser for thick plate welding. A 16 kW disk laser was used for single-pass welding of 15 mm thick plates in a butt joint configuration. Root humping occurred within a wide range of welding parameters. This provides narrow processing window. By adding an arc source to the laser beam process, the tendency of root humping increases. To achieve humping-free welds and consistent root quality over length, a delicate balance of process parameters is required. High heat input (> 0.50 kJ/mm) was positive to achieve a combination of low hardness (< 325 HV) and good Charpy toughness at -50 °C (> 50 J).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.