Abstract

A wear-resistant alloy consisting of Cr13Ni5Si2 ternary silicide dendrites and the interdendritic nickel-base solid solution (γ) was designed and fabricated by the laser melting/continuous deposition (LMCD) process. The wear resistance of Cr13Ni5Si2/γ alloy was evaluated on an MM-200 block-on-wheel dry sliding wear tester at room temperature. Results indicate that the Cr13Ni5Si2/γ alloy has excellent wear resistance and extremely low load-sensitivity of wear under dry sliding wear test conditions due to the high toughness and the high strength, as well as the transferred cover-layer on the worn surface of the alloy.