Abstract

AbaCus, a newly developed fluorine-free precursor has been used for room temperature copper deposition using plasma enhanced chemical vapor deposition (PEALD). This process has been characterized and the film properties investigated in term of composition, deposition rate, resistivity, grain size and platability. Integration results with completely filled structures obtained demonstrate a high potential for use in advanced interconnect technologies.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.