Abstract
Fe-3.10%Si thin strips were prepared from commercial grain oriented silicon steel sheet by cold rolling with different speed ratios and annealed at 1123K in vacuum, the cold rolling and recrystallization textures were analyzed. Cold rolling texture consists mainly of {111}<112>, {554}<225> and {332}<113> components, while their orientation densities vary with speed ratio and layer through strip thickness. Recrystallization texture development depends on speed ratio obviously, and the peak orientation density deviates from {110}<001> towards {210}<001> with the increase in speed ratio.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.