Abstract Paint delamination from cut edges of model coil coated hot dip galvanized materials exposed at a marine test site for 5 years increased with steel thickness and decreased with zinc coating thickness. It was larger in sheltered locations than for openly exposed cut edges whereas red rust protection was more efficient on sheltered edges due to higher electric conductivity of deposits. The rate of paint delamination increased or decreased in time depending on the relative amount of zinc ions available for formation of the protective film on steel controlled by the initial steel substrate and zinc coating thicknesses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.