Abstract

Photo-pumped lasing properties have been investigated in a CdSe/ZnSe/ZnSSE single quantum wells (SQWs) with the well-layer thickness (LW) of 1, 2 and 3 monolayer (ML). At 20 K, the laser threshold for the SQW withLW= 1 ML was the lowest in spite of the smallest active layer thickness. The carrier (exciton) sheet density at the threshold (n)thwas estimated to be as low as 7 × 1010cm−2, which is well below Mott's screening density. Time-resolved photoluminescence has revealed that the localized biexciton band, whose peak energy agrees with the lasing peak, appeared on the low-energy side of the main PL peak at this level of carrier concentrations. Theoretical calculation has also shown that the localized biexciton recombination has to be taken into account for the lasing process. On the contrary, thenthvalues of the SQWs with 2 and 3 ML are 1 order of magnitude larger than that of the SQW with 1 ML. This may be due to the smaller oscillator strength of both localized excitons and localized biexcitons because of the larger inhomogeneous broadening, resulting in an increased carrier density for achieving optical gain sufficient to overcome the reflection losses.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.