Abstract

Anisotropic Pr13Fe80B7 magnetic powders are obtained by shortening the disproportionation time of the hydrogenation disproportionation desorption recombination (HDDR) process. The magnetic powders with a disproportionation time of 30 min have the magnetic properties of Br=0.93 T and Mr/Ms=0.75, and show a high degree of crystal texture along the c axis, whereas the magnetic powders obtained with a prolonged disproportionation time are isotropic. A rodlike structure is observed in the 30 min-disproportionation products and is transformed into spherical morphology with a prolonged disproportionation time. It suggests that the rodlike disproportionated microstructure is very important for the formation of crystal texture in the conventional HDDR powders.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.