The durability of concrete repair may be measured in terms of its resistance to cracking and to ingress by aggressive species. This paper addresses the various issues that form the nucleus of cracking resistance, including the role of material parameter indices such as free drying shrinkage and specific tensile creep. Data for these indices are presented for two new generation repair materials, and attention is drawn to the inherent anomalies existing in international specifications for shrinkage measurement. The paper concludes by defining risk factors associated with the probability of failure of a patch repair in one of three identified modes. The risk factors are computed for a patch repair using a rigid substrate idealization, and the probability of failure in cracking, delamination, or peeling modes is assessed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.